摘    要:试样在650℃烧制、王水溶解、泡塑振荡吸附、硫脲解脱,用电感耦合等离子体发射光谱法测定矿石中的金量,克服了原子吸收光谱法对低含量金测定稳定性和精密度差、对高含量金测定分取误差大和返工率高等不足,缩短了分析时间。方法经国家一级标准物质分析验证,结果与标准值相符。对二级标准物质测定的方法精密度(RSD,n=12)为6.45%。方法检出限为0.138μg/g,线性范围宽,适用于矿石中0.2μg/g以上金的测定。

关 键 词:电感耦合等离子体发射光谱法  王水溶解  泡塑吸附  硫脲解脱    矿石
收稿时间:2008/7/31 0:00:00
修稿时间:2008/10/6 0:00:00

Determination of Gold in Ores by Inductively Coupled Plasma-Atomic Emission Spectrometry with Plastic Foam Absorption
TAN Jian-an,HEI Wen-long,HUANG Xing-hua and CHEN Yue-yuan.Determination of Gold in Ores by Inductively Coupled Plasma-Atomic Emission Spectrometry with Plastic Foam Absorption[J].Rock and Mineral Analysis,2009,28(2):147-150.
Authors:TAN Jian-an  HEI Wen-long  HUANG Xing-hua and CHEN Yue-yuan
Affiliation:(Lanzhou Testing and Quality Supervision Center for Geological and Mineral Products,The Ministry of Land and Resources,Lanzhou 730050,China)
Abstract:Ore sample,pretreated at 650℃,was decomposed with aqua regia.Au in the sample solution was then pre-concentrated by adsorbing with polyurethane foam plastic and released with thiourea solution and determined by inductively coupled plasma-atomic emission spectrometry.The detection limit of the method for Au was 0.138 μg/g.The method has been applied to determination of Au in National Standard Reference materials and the results are in agreement with certified values with precision of 6.45%RSD(n=12).The method provides the advantages of higher stability,higher accuracy and more efficiency compared with atomic absorption spectrometry(AAS).
Keywords:inductively coupled plasma-atomic emission spectrometry  aqua regia dissolution  plastic foam absorption  thiourea elution  gold  ore
本文献已被 CNKI 维普 万方数据 等数据库收录!